Term
The stress at which plastic deformation begins is called the |
|
Definition
|
|
Term
The stress at which the maximum force that can be withstood by either a ductile or a brittle material is called the |
|
Definition
|
|
Term
The slope of the stress-strain curve, which is determined primarily by the strength of the atomic bonds within the material, is called the |
|
Definition
|
|
Term
When you design a part or select a material for a given application, you almost always want to be sure that the stress acting on the material during its service |
|
Definition
is below the yield strength |
|
|
Term
Necking of a ductile material occurs when the applied stress |
|
Definition
reaches the tensile strength |
|
|
Term
The stiffness of a material is most closely related to |
|
Definition
the modulus of elasticity |
|
|
Term
For a given applied force, we expect that the true stress acting on a material will be |
|
Definition
higher than the engineering stress |
|
|
Term
almost always, as the temperature increases, |
|
Definition
|
|
Term
|
Definition
the elastic portion of a stress-strain curve |
|
|
Term
We would expect that the percent reduction in area will be larger for a material that |
|
Definition
breaks after a large amount of necking has occured |
|
|
Term
If we want to shape a metal into a complex part by bending, forging, or some other metal-working process, we must |
|
Definition
always be sure that the stress applied during the metal working process is above the yield strength |
|
|
Term
Which hardness test measures the depth of penetration to determine the hardness of a material? |
|
Definition
|
|
Term
The tensile strength of a steel specimen with a measured hardness of 240 BHN is approximately |
|
Definition
|
|
Term
When a component possesses a flat fracture with little or no plastic deformation, it is said to have fractured by which of the following |
|
Definition
|
|
Term
An irregular, granular appearance on a fracture surface is normally indicative of which type of fracture? |
|
Definition
|
|
Term
Chevron markings and radial lines typically occur with which of the following types of fracture? |
|
Definition
|
|
Term
Chevron markings on a component point back to |
|
Definition
The point of initiation of the crack |
|
|
Term
Beach marks are commonly seen on which type of fracture surface? |
|
Definition
|
|
Term
Each striation on a fracture surface corresponds with one loading cycle. |
|
Definition
|
|
Term
Striations are visible with the naked eye. |
|
Definition
|
|
Term
Particularly in brittle fracture, the crack propagates in a direction |
|
Definition
perpendicular to the applied tensile stress |
|
|
Term
A ductile cup-and-cone fracture is typically produced |
|
Definition
through microvoid coalescence |
|
|
Term
The plane strain fracture toughness K1c is |
|
Definition
|
|
Term
Which of the following is not a factor that affects whether or not a material will fracture in a ductile or brittle manner? |
|
Definition
all of these affect the mode of fracture |
|
|
Term
Because of the nature of impact testing |
|
Definition
the data should only be used qualitatively in design |
|
|
Term
One of the most important properties obtained through impact testing is |
|
Definition
the ductle-brittle transition temperature |
|
|
Term
In which of the following metals would we not expect to see a ductile-brittle transition? |
|
Definition
|
|
Term
One method to improve the fatigue life of a component is to |
|
Definition
Impart residual compressive stresses at the surface of the part. |
|
|